Ranu Ranu Rubber Ceramic Matrix
MO TE Ranu Ranu Rubber Ceramic Matrix
Ka honohia ma te whakamahi i tetahi tukanga motuhake, ka whakakotahihia e te Hybrid Liner nga rauemi raina e rua me o raatau ahuatanga pai.Ko te roto he mea hanga ki te polyurethane me te tiaki i te toenga o nga peka me nga hanganga wheua na runga i ona ahuatanga ohorere.I te wa ano, ka whakapumau i te tohatoha pehanga tino pai puta noa i te toenga o te toenga, mo te whakatipuranga haruru me te hohe o te korehau.Ko te waho o te riipene me te papa korehau whakauru he mea hanga ki te silicone, kua whakamatauhia i roto i nga mahi o ia ra na tona kaha.He mea tino nui tenei ina ka takai te papa korehau ki runga i te turanga o roto hei hanga hiri hau mo te punaha.
Ranu Ranu Rubber Ceramic Matrix Taupānga
Mo runga mo te abrasion e pa ana ki nga arai rapa, me whakaaro nga korero e whai ake nei.
1- E rua nga momo abrasion ka pa ki tetahi, ko te wero me te paheke.
2- Ka puta te abrasion impingement ina pa ana matūriki te mata o te rapa (tetahi atu mata ranei).
3- Ka paheke te abrasion ka paheke tetahi atu mata puta noa i te rapa.
4- I roto i nga ahuatanga katoa ka taea te whakaaro ko te abrasion he huinga o te wero me te retireti.
5- Ko te nuinga o te wa ka puta te abrasion ki roto i nga chutes, ngongo kirikiri me nga waahi katoa ka kitea te hokinga mai.
6- I roto i te mahi whakangao, ka pa te matūriki ki te mata, ka tohatohahia nga taumahatanga ka puta mena ka ngawari te hua o te rapa, ina koa ka pa te matūriki i te koki 90° ki te mata.
Nga Rawa Maama (Alumina + Tauhohenga Tile Silicon Carbide)
Kāwai | 92% Al2O3 | 95% Al2O3 |
ZrO2 | / | / |
Kiato(gr/cm3) | >3.60 | >3.65g |
HV 20 | ≥950 | ≥1000 |
Rock Hardness HRA | ≥82 | ≥85 |
Te Kaha Piko MPa | ≥220 | ≥250 |
Kaha kōpeketanga MPa | ≥1050 | ≥1300 |
Maamaa Whati (KIc MPam 1/2) | ≥3.7 | ≥3.8 |
Whakamau Rōrahi (cm3) | ≤0.25 | ≤0.20 |
Silicon CarbideRaraunga(RBSiC) | ||
Taurangi | Uara | Hua whakamātautau |
Sic | / | ≧90 |
Te pāmahana | ℃ | 1380 |
Kiatotanga Tauwhāiti | g/cm3 | ≧3.02 |
Porosity Tuwhera | % | <0.1 |
Kōwae o te elasticity: | Gpa | 330Gpa (20℃) 300Gpa(1200 ℃) |
Te pakeke o Moh | / | 9.6 |
Te kaha piko | Mpa | 250(20℃)/280 (1200℃) |
Kaha Kōpeketanga | Mpa | 1150 |
Te whakarea o te roha wera: | / | 4.5K^(-3)*10^(-5) |
Te whakarea o te kawe werawera: | W/mk | 45 (1200 ℃) |
Waikawa Waikawa -tohu | / | Tino pai |